| Plate |
Highly recommended for Durable Thermal Positive Plate
DTP150, Durable Thermal Positive Plate DTP150i,Durable Thermal
Positive Plate DTP150eu and Durable Thermal Positive Plate
DTP150i+
|
| Application |
Development in processors for thermal plates. Direction for use |
| Specifications |
pH value above 13 and Conductivity between 84 to 86 mS at 25oC |
| Working temperature |
23oC ± 1oC |
| Developer time |
30 ± 5 seconds in immersion2
|
| Replenishment |
Use Thermal Positive Plate Replenisher GSP100 |
| Replenishment rate |
80 ÷ 90 ml/m2
|
| Antioxidant Stand by ON |
50 ml/h |
| Antioxidant Stand by OFF |
50 ml/h |
| Considerations |
Adequate replenishment keeps filters and circulation systems clean
prolonging the life of the bath. Correct cleaning of the equipment will avoid
contamination of the new bath and prolong the life of the processor.
|
| Safelight |
None required - daylight handling |
| Shelf life |
12 months under recommended storage conditions
|
| Packaging |
10, 20 liters
|
| Transport and storage |
Should be stored flat and away from excessive cold, heat and humidity.
Use in a controlled environment of 5oC - 30oC and 40 - 80% RH, non-
condensing
|
| Availability |
Contact your local MyLan Group representative. See the list of our Distributors at www.mylangroup.com for contact information.
|
|
|